A Fractographic Study of BendingTorsion Fatigue Failure in Metallic Materials with Protective Surface Layers
المؤلفون المشاركون
Šesták, Petr
Slámečka, Karel
Vojtek, Tomáš
Kianicová, Marta
Horníková, Jana
Šandera, Pavel
Pokluda, Jaroslav
المصدر
Advances in Materials Science and Engineering
العدد
المجلد 2016، العدد 2016 (31 ديسمبر/كانون الأول 2016)، ص ص. 1-6، 6ص.
الناشر
Hindawi Publishing Corporation
تاريخ النشر
2016-06-09
دولة النشر
مصر
عدد الصفحات
6
الملخص EN
Results are given of a fractographic study of biaxial in-phase bending/torsion fatigue fractures in specimens made of nitrided steel and nickel-based superalloy with protective coatings (diffusion coatings and plasma-sprayed thermal barrier coatings).
Fracture surfaces were examined by optical and scanning electron microscopes while stereophotogrammetry and optical profilometry were employed to obtain 3D surface data of selected fracture surface regions.
The studied materials exhibited a wide range of fracture mechanisms depending on the microstructure and applied mechanical loading.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Slámečka, Karel& Šesták, Petr& Vojtek, Tomáš& Kianicová, Marta& Horníková, Jana& Šandera, Pavel…[et al.]. 2016. A Fractographic Study of BendingTorsion Fatigue Failure in Metallic Materials with Protective Surface Layers. Advances in Materials Science and Engineering،Vol. 2016, no. 2016, pp.1-6.
https://search.emarefa.net/detail/BIM-1096461
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Slámečka, Karel…[et al.]. A Fractographic Study of BendingTorsion Fatigue Failure in Metallic Materials with Protective Surface Layers. Advances in Materials Science and Engineering No. 2016 (2016), pp.1-6.
https://search.emarefa.net/detail/BIM-1096461
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Slámečka, Karel& Šesták, Petr& Vojtek, Tomáš& Kianicová, Marta& Horníková, Jana& Šandera, Pavel…[et al.]. A Fractographic Study of BendingTorsion Fatigue Failure in Metallic Materials with Protective Surface Layers. Advances in Materials Science and Engineering. 2016. Vol. 2016, no. 2016, pp.1-6.
https://search.emarefa.net/detail/BIM-1096461
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes bibliographical references
رقم السجل
BIM-1096461
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر