Enhancement of EDM performance by using copper-silver composite electrode

المؤلفون المشاركون

Shadhar, Sad Karim
Muhsins, Zaynab H.
Hassun, Umar H.
Ibrahim, Abbas F.

المصدر

Engineering and Technology Journal

العدد

المجلد 38، العدد 9A (30 سبتمبر/أيلول 2020)، ص ص. 1352-1358، 7ص.

الناشر

الجامعة التكنولوجية

تاريخ النشر

2020-09-30

دولة النشر

العراق

عدد الصفحات

7

التخصصات الرئيسية

هندسة المواد والمعادن
الهندسة الكهربائية

الموضوعات

الملخص EN

Discharge Machining is a non-traditional machining technique and usually applied for hard metals and complex shapes that difficult to machining in the traditional cutting process.

This process depends on different parameters that can affect the material removal rate and surface roughness.

The electrode material is one of theimportant parametersin Electro –Discharge Machining (EDM).

In this paper, the experimental work carried out by using a composite materialelectrodeand the workpiece material from a high-speed steel plate.

The cutting conditions: current (10 Amps, 12 Amps, 14 Amps), pulse on time (100 μs, 150 μs, 200 μs), pulse off time 25 μs, casting technique has been carried out to prepare the composite electrodes copper-sliver.

The experimental results showed that Copper-Sliver (weight ratio70: 30) givesbetter results than commonly electrode copper, Material Removal Rate (MRR) Copper-Sliver composite electrode reach to 0.225 gm/min higher than the pure Copper electrode.

The lower value of the tool wear rate achieved with the composite electrode is 0.0001 gm/min.

The surface roughness of the workpiece improved with a composite electrode compared with the pure on different parameters that can affect the material removal rate and surface roughness.

The electrode material is one of theimportant parametersin Electro –Discharge Machining (EDM).

In this paper, the experimental work carried out by using a composite materialelectrodeand the workpiece material from a high-speed steel plate.

The cutting conditions: current (10 Amps, 12 Amps, 14 Amps), pulse on time (100 μs, 150 μs, 200 μs), pulse off time 25 μs, casting technique has been carried out to prepare the composite electrodes copper-sliver.

The experimental results showed that Copper-Sliver (weight ratio70: 30) givesbetter results than commonly electrode copper, Material Removal Rate (MRR) Copper-Sliver composite electrode reach to 0.225 gm/min higher than the pure Copper electrode.

The lower value of the tool wear rate achieved with the composite electrode is 0.0001 gm/min.

The surface roughness of the workpiece improved with a composite electrode compared with the pure electrode.

نمط استشهاد جمعية علماء النفس الأمريكية (APA)

Shadhar, Sad Karim& Ibrahim, Abbas F.& Muhsins, Zaynab H.& Hassun, Umar H.. 2020. Enhancement of EDM performance by using copper-silver composite electrode. Engineering and Technology Journal،Vol. 38, no. 9A, pp.1352-1358.
https://search.emarefa.net/detail/BIM-1236317

نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)

Shadhar, Sad Karim…[et al.]. Enhancement of EDM performance by using copper-silver composite electrode. Engineering and Technology Journal Vol. 38, no. 9A (2020), pp.1352-1358.
https://search.emarefa.net/detail/BIM-1236317

نمط استشهاد الجمعية الطبية الأمريكية (AMA)

Shadhar, Sad Karim& Ibrahim, Abbas F.& Muhsins, Zaynab H.& Hassun, Umar H.. Enhancement of EDM performance by using copper-silver composite electrode. Engineering and Technology Journal. 2020. Vol. 38, no. 9A, pp.1352-1358.