Time Dependent Development of Aluminium Pitting Corrosion
المؤلف
المصدر
Advances in Materials Science and Engineering
العدد
المجلد 2015، العدد 2015 (31 ديسمبر/كانون الأول 2015)، ص ص. 1-10، 10ص.
الناشر
Hindawi Publishing Corporation
تاريخ النشر
2015-05-28
دولة النشر
مصر
عدد الصفحات
10
الملخص EN
Aluminium alloys have excellent corrosion resistance to a wide variety of exposure conditions.
Usually they corrode by pitting rather than by uniform corrosion.
For infrastructure applications long-term corrosion behaviour is of interest.
The relatively limited long-term pitting data that is available shows that maximum and average pit depths do not follow the power law function as conventionally assumed but tend to follow a bimodal trend with exposure time.
This is consistent with the bimodal trends observed previously for corrosion mass loss of aluminium alloys.
Most likely it is the result of the accumulation of corrosion products over the pit mouths, leading to the gradual development of localised anoxic conditions within pits.
In turn this permits the development within the pits of anoxic autocatalytic conditions, consistent with established theory for pitting corrosion of aluminium.
It also is consistent with observations of hydrogen evolution from pits.
The implications of this for practical applications are discussed.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Melchers, Robert E.. 2015. Time Dependent Development of Aluminium Pitting Corrosion. Advances in Materials Science and Engineering،Vol. 2015, no. 2015, pp.1-10.
https://search.emarefa.net/detail/BIM-1053126
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Melchers, Robert E.. Time Dependent Development of Aluminium Pitting Corrosion. Advances in Materials Science and Engineering No. 2015 (2015), pp.1-10.
https://search.emarefa.net/detail/BIM-1053126
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Melchers, Robert E.. Time Dependent Development of Aluminium Pitting Corrosion. Advances in Materials Science and Engineering. 2015. Vol. 2015, no. 2015, pp.1-10.
https://search.emarefa.net/detail/BIM-1053126
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes bibliographical references
رقم السجل
BIM-1053126
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر