Properties of GH4169 Superalloy Characterized by Nonlinear Ultrasonic Waves
المؤلفون المشاركون
Yan, Hongjuan
Xu, Chunguang
Xiao, Dingguo
Cai, Haichao
المصدر
Advances in Materials Science and Engineering
العدد
المجلد 2015، العدد 2015 (31 ديسمبر/كانون الأول 2015)، ص ص. 1-8، 8ص.
الناشر
Hindawi Publishing Corporation
تاريخ النشر
2015-02-17
دولة النشر
مصر
عدد الصفحات
8
الملخص EN
The nonlinear wave motion equation is solved by the perturbation method.
The nonlinear ultrasonic coefficients β and δ are related to the fundamental and harmonic amplitudes.
The nonlinear ultrasonic testing system is used to detect received signals during tensile testing and bending fatigue testing of GH4169 superalloy.
The results show that the curves of nonlinear ultrasonic parameters as a function of tensile stress or fatigue life are approximately saddle.
There are two stages in relationship curves of relative nonlinear coefficients β′ and δ′ versus stress and fatigue life.
The relative nonlinear coefficients β′ and δ′ increase with tensile stress when tensile stress is lower than 65.8% of the yield strength, and they decrease with tensile stress when tensile stress is higher than 65.8% of the yield strength.
The nonlinear coefficients have the extreme values at 53.3% of fatigue life.
For the second order relative nonlinear coefficient β′, there is good agreement between the experimental data and the comprehensive model.
For the third order relative nonlinear coefficient δ′, however, the experiment data does not accord with the theoretical model.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Yan, Hongjuan& Xu, Chunguang& Xiao, Dingguo& Cai, Haichao. 2015. Properties of GH4169 Superalloy Characterized by Nonlinear Ultrasonic Waves. Advances in Materials Science and Engineering،Vol. 2015, no. 2015, pp.1-8.
https://search.emarefa.net/detail/BIM-1053302
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Yan, Hongjuan…[et al.]. Properties of GH4169 Superalloy Characterized by Nonlinear Ultrasonic Waves. Advances in Materials Science and Engineering No. 2015 (2015), pp.1-8.
https://search.emarefa.net/detail/BIM-1053302
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Yan, Hongjuan& Xu, Chunguang& Xiao, Dingguo& Cai, Haichao. Properties of GH4169 Superalloy Characterized by Nonlinear Ultrasonic Waves. Advances in Materials Science and Engineering. 2015. Vol. 2015, no. 2015, pp.1-8.
https://search.emarefa.net/detail/BIM-1053302
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes bibliographical references
رقم السجل
BIM-1053302
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر