Study on Application of Grey Prediction Model in Superalloy MAR-247 Machining
المؤلف
المصدر
Advances in Materials Science and Engineering
العدد
المجلد 2015، العدد 2015 (31 ديسمبر/كانون الأول 2015)، ص ص. 1-10، 10ص.
الناشر
Hindawi Publishing Corporation
تاريخ النشر
2015-09-07
دولة النشر
مصر
عدد الصفحات
10
الملخص EN
Superalloy MAR-247 is mainly applied in the space industry and die industry.
With its characteristics of mechanical property, fatigue resistance, and high temperature corrosion resistance, therefore, it is mainly applied in machine parts of high temperature and corrosion resistance, such as turbine blades and rotor of the aeroengine and turbine assembly in the nuclear power plant.
However, considering that its properties of high strength, low thermal conductivity, being difficult to soften, and work hardening may reduce the life of cutting-tool and weaken the surface accuracy, the study provided minimizing experiment occurring during milling process for superalloy material.
As a statistical approach used to analyse experiment data, this study used GM(1,1) in the grey prediction model to conduct simulation and then predict and analyze its characteristics based on the experimental data, focusing on the tool life and surface accuracy.
Moreover, with the superalloy machining parameters of the current effective application improved grey prediction model, it can decrease the errors, extend the tool life, and improve the prediction precision of surface accuracy.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Chen, Shao-Hsien. 2015. Study on Application of Grey Prediction Model in Superalloy MAR-247 Machining. Advances in Materials Science and Engineering،Vol. 2015, no. 2015, pp.1-10.
https://search.emarefa.net/detail/BIM-1053629
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Chen, Shao-Hsien. Study on Application of Grey Prediction Model in Superalloy MAR-247 Machining. Advances in Materials Science and Engineering No. 2015 (2015), pp.1-10.
https://search.emarefa.net/detail/BIM-1053629
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Chen, Shao-Hsien. Study on Application of Grey Prediction Model in Superalloy MAR-247 Machining. Advances in Materials Science and Engineering. 2015. Vol. 2015, no. 2015, pp.1-10.
https://search.emarefa.net/detail/BIM-1053629
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes bibliographical references
رقم السجل
BIM-1053629
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر