We present a user-friendly vision-augmented technique to carry out atomic simulation using hand gestures.
The system is novel in its concept as it enables the user to directly manipulate the atomic structures on the screen, in 3D space using hand gestures, allowing the exploration and visualisation of molecular interactions at different relative conformations.
The hand gestures are used to pick and place atoms on the screen allowing thereby the ease of carrying out molecular dynamics simulation in a more efficient way.
The end result is that users with limited expertise in developing molecular structures can now do so easily and intuitively by the use of body gestures to interact with the simulator to study the system in question.
The proposed system was tested by simulating the crystal anisotropy of crystalline silicon during nanoindentation.
A long-range (Screened bond order) Tersoff potential energy function was used during the simulation which revealed the value of hardness and elastic modulus being similar to what has been found previously from the experiments.
We anticipate that our proposed system will open up new horizons to the current methods on how an MD simulation is designed and executed.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Al-Sayegh, Rajab& Makatsoris, Charalampos. 2015. Vision-Augmented Molecular Dynamics Simulation of Nanoindentation. Journal of Nanomaterials،Vol. 2015, no. 2015, pp.1-11.
https://search.emarefa.net/detail/BIM-1069381
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Al-Sayegh, Rajab& Makatsoris, Charalampos. Vision-Augmented Molecular Dynamics Simulation of Nanoindentation. Journal of Nanomaterials No. 2015 (2015), pp.1-11.
https://search.emarefa.net/detail/BIM-1069381
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Al-Sayegh, Rajab& Makatsoris, Charalampos. Vision-Augmented Molecular Dynamics Simulation of Nanoindentation. Journal of Nanomaterials. 2015. Vol. 2015, no. 2015, pp.1-11.
https://search.emarefa.net/detail/BIM-1069381
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes bibliographical references
رقم السجل
BIM-1069381
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر