الملخص EN

The purpose of this study was to evaluate the fracture load of two CAD/CAM ceramic veneer materials (IPS Empress CAD and IPS e-max CAD), with three different preparation designs (window, butt-joint, and incisal overlap).

Thirty maxillary anterior teeth were restored with ceramic laminate veneers and divided into 6 groups as follows: group I-A (laminates made of IPS Empress CAD with window preparation design), group I-B (laminates made of IPS Empress CAD with butt-joint preparation design), group I-C (laminates made of IPS Empress CAD with incisal overlap preparation design), group II-A (laminates made of IPS e-max CAD with window preparation design), group II-B (laminates made of IPS e-max CAD with butt-joint preparation design), group II-C (laminates made of IPS e-max CAD with incisal overlap preparation design).

Fracture load test was performed using the Universal Testing Machine (UTM).

Data were statistically analyzed using One-way analysis of variance ANOVA followed by Tukey’s multiple comparison test.

The results of the fracture load test were recorded in Newton: (I-A: 233.7 N); (I-B: 252.1 N); (I-C: 200.3 N); (II-A: 227.6 N); (II-B: 283.5 N); (II-C: 256.7 N).

Statistical analysis showed that the result of the butt-joint design (II-B) was significantly higher than other subgroups, and regarding the materials used, the IPS e-max CAD was significantly higher than the IPS Empress CAD material in fracture load test.

نمط استشهاد جمعية علماء النفس الأمريكية (APA)

Khatib, Dua& Qatamish, Hisham& Ibrahim, Atif Shakir. 2009. Fracture load of two CADCAM ceramic veneers with different preparation designs. Cairo Dental Journal،Vol. 25, no. 3, pp.425-432.
https://search.emarefa.net/detail/BIM-274073

نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)

Khatib, Dua…[et al.]. Fracture load of two CADCAM ceramic veneers with different preparation designs. Cairo Dental Journal Vol. 25, no. 3 (Sep. 2009), pp.425-432.
https://search.emarefa.net/detail/BIM-274073

نمط استشهاد الجمعية الطبية الأمريكية (AMA)

Khatib, Dua& Qatamish, Hisham& Ibrahim, Atif Shakir. Fracture load of two CADCAM ceramic veneers with different preparation designs. Cairo Dental Journal. 2009. Vol. 25, no. 3, pp.425-432.
https://search.emarefa.net/detail/BIM-274073

نوع البيانات

مقالات

لغة النص

الإنجليزية

الملاحظات

Includes bibliographical references : p. 431-432

رقم السجل

BIM-274073