![](/images/graphics-bg.png)
Improvement of Pitting Corrosion Resistance of Type 316L Stainless Steel by Potentiostatic Removal of Surface MnS Inclusions
المؤلفون المشاركون
Sugawara, Yu
Hirabayashi, Koichi
Muto, Izumi
Hara, Nobuyoshi
المصدر
International Journal of Corrosion
العدد
المجلد 2012، العدد 2012 (31 ديسمبر/كانون الأول 2012)، ص ص. 1-6، 6ص.
الناشر
Hindawi Publishing Corporation
تاريخ النشر
2012-07-05
دولة النشر
مصر
عدد الصفحات
6
التخصصات الرئيسية
الملخص EN
The beneficial effect of the removal of MnS inclusions on the pitting of stainless steels has been demonstrated in two ways.
(1) High-purity Type 316L stainless steel with no inclusions was used as a specimen in the measurement of anodic polarization curves in 0.5 M NaCl and (2) commercial Type 316L stainless steel with MnS and slag-related inclusions was first polarized at different potentials for 30 min in 1 M Na2SO4 of pH 3 and then anodic polarization measurements were taken in 0.5 M NaCl.
Pitting did not occur in the passive or transpassive region of the high-purity steel.
The polarization treatment dissolved MnS and some oxide inclusions (CaO and SiO2) on the surface of the commercial steel.
An increase in pitting potential of the commercial steel was noted after treatment at potentials above 0.2 V.
At the same time, the number of current spikes due to metastable pits decreased significantly.
These results are more likely due to the beneficial effect of removing MnS inclusions from the steel surface rather than the modification effect of the chemical composition of passive films on the surface.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Hara, Nobuyoshi& Hirabayashi, Koichi& Sugawara, Yu& Muto, Izumi. 2012. Improvement of Pitting Corrosion Resistance of Type 316L Stainless Steel by Potentiostatic Removal of Surface MnS Inclusions. International Journal of Corrosion،Vol. 2012, no. 2012, pp.1-6.
https://search.emarefa.net/detail/BIM-475128
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Hara, Nobuyoshi…[et al.]. Improvement of Pitting Corrosion Resistance of Type 316L Stainless Steel by Potentiostatic Removal of Surface MnS Inclusions. International Journal of Corrosion No. 2012 (2012), pp.1-6.
https://search.emarefa.net/detail/BIM-475128
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Hara, Nobuyoshi& Hirabayashi, Koichi& Sugawara, Yu& Muto, Izumi. Improvement of Pitting Corrosion Resistance of Type 316L Stainless Steel by Potentiostatic Removal of Surface MnS Inclusions. International Journal of Corrosion. 2012. Vol. 2012, no. 2012, pp.1-6.
https://search.emarefa.net/detail/BIM-475128
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes bibliographical references
رقم السجل
BIM-475128
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
![](/images/ebook-kashef.png)
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر
![](/images/kashef-image.png)