Galvanic corrosion of carbon steel -stainless steel couple in sulfuric acid under flow conditions
العناوين الأخرى
التآكل الكلفاني للحديد الكاربوني و الحديد المقاوم للصدأ في حامض الكبريتيك تحت تاثير الجريان
المؤلفون المشاركون
Hasan, Basim Ubayd
Husayn, Samar Sadi
al-Habubi, Nusayr Abbud
المصدر
العدد
المجلد 22، العدد 8 (31 أغسطس/آب 2016)، ص ص. 158-174، 17ص.
الناشر
تاريخ النشر
2016-08-31
دولة النشر
العراق
عدد الصفحات
17
التخصصات الرئيسية
الملخص EN
Galvanic corrosion of stainless steel 316 (SS316) and carbon steel (CS) coupled in 5% wt/v sulfuric acid solution at agitation velocity was investigated.
The galvanic behavior of coupled metals was also studies using zero resistance ammeter (ZRA) method.
The effects of agitation velocity, temperature, and time on galvanic corrosion current and loss in weight of both metals in both free corrosion and galvanic corrosion were investigated.
The trends of open circuit potential (OCP) of each metal and galvanic potential (Eg) of the couple were, also, determined.
Results showed that SS316 was cathodic relative to CS in galvanic couple and its OCP was much more positive than that of CS for all investigated ranges of operating conditions.
A sharp increase in galvanic current from CS to SS316 in the first 20 min and then decrease with time.
Increasing the agitation velocity led to increase in galvanic corrosion rate.
The decrease in galvanic current is attributed to metal passivation due to the formation of a protective film which grows with time.
The minus sign in galvanic current means that the current is flow from CS (anode) to SS316 (Cathode).
The galvanic current of CS-SS316 couple shifts to the negative direction with increase agitation velocity.
نمط استشهاد جمعية علماء النفس الأمريكية (APA)
Hasan, Basim Ubayd& al-Habubi, Nusayr Abbud& Husayn, Samar Sadi. 2016. Galvanic corrosion of carbon steel -stainless steel couple in sulfuric acid under flow conditions. Journal of Engineering،Vol. 22, no. 8, pp.158-174.
https://search.emarefa.net/detail/BIM-708537
نمط استشهاد الجمعية الأمريكية للغات الحديثة (MLA)
Hasan, Basim Ubayd…[et al.]. Galvanic corrosion of carbon steel -stainless steel couple in sulfuric acid under flow conditions. Journal of Engineering Vol. 22, no. 8 (Aug. 2016), pp.158-174.
https://search.emarefa.net/detail/BIM-708537
نمط استشهاد الجمعية الطبية الأمريكية (AMA)
Hasan, Basim Ubayd& al-Habubi, Nusayr Abbud& Husayn, Samar Sadi. Galvanic corrosion of carbon steel -stainless steel couple in sulfuric acid under flow conditions. Journal of Engineering. 2016. Vol. 22, no. 8, pp.158-174.
https://search.emarefa.net/detail/BIM-708537
نوع البيانات
مقالات
لغة النص
الإنجليزية
الملاحظات
Includes appendices : p. 167-174
رقم السجل
BIM-708537
قاعدة معامل التأثير والاستشهادات المرجعية العربي "ارسيف Arcif"
أضخم قاعدة بيانات عربية للاستشهادات المرجعية للمجلات العلمية المحكمة الصادرة في العالم العربي
تقوم هذه الخدمة بالتحقق من التشابه أو الانتحال في الأبحاث والمقالات العلمية والأطروحات الجامعية والكتب والأبحاث باللغة العربية، وتحديد درجة التشابه أو أصالة الأعمال البحثية وحماية ملكيتها الفكرية. تعرف اكثر