Evaluation of the Loading, Unloading, and Permanent Deformation of Newly Available Epoxy Resin Coated Ni-Ti Wires Using Self-Ligating Brackets

Joint Authors

Garro-Piña, Hazel
Jiménez-Cervantes, María Cristina
Ondarza-Rovira, Ricardo
Justus, Roberto
García-López, Salvador

Source

International Journal of Dentistry

Issue

Vol. 2017, Issue 2017 (31 Dec. 2017), pp.1-8, 8 p.

Publisher

Hindawi Publishing Corporation

Publication Date

2017-05-23

Country of Publication

Egypt

No. of Pages

8

Main Subjects

Dental

Abstract EN

Aim.

The purpose of this study was to evaluate the load and unload deflection and permanent deformation of round 0.016′′ and rectangular 0.016′′×0.022′′ regular and coated Ni-Ti wires.

Materials and Methods.

Ni-Ti archwires produced by two manufacturers were evaluated.

Both regular and coated round and rectangular Ni-Ti wire segments (n=15) from each group were submitted to a three-point bending test.

Both types of wires were evaluated for permanent deformation at the end of a recovery cycle.

Results.

The coated round 0.016′′ Ni-Ti wires produced a significantly lower force in loading (p<0.01) and unloading (p<0.01) than regular wires of the same manufacturer and size.

There was no significant difference in permanent deformation between coated and regular round Ni-Ti wires from the same company.

For rectangular 0.016×0.022′′ Ni-Ti wires, there was a significant difference in the loading evaluation, but the unloading test presented no significant differences.

The permanent deformation of the rectangular wires revealed no significant difference between them.

Conclusion.

The addition of an esthetic coating to these new Ni-Ti wires produced changes in their mechanical properties, manifested as a reduction in the applied force, which should be considered in clinical management.

American Psychological Association (APA)

Garro-Piña, Hazel& Jiménez-Cervantes, María Cristina& Ondarza-Rovira, Ricardo& Justus, Roberto& García-López, Salvador. 2017. Evaluation of the Loading, Unloading, and Permanent Deformation of Newly Available Epoxy Resin Coated Ni-Ti Wires Using Self-Ligating Brackets. International Journal of Dentistry،Vol. 2017, no. 2017, pp.1-8.
https://search.emarefa.net/detail/BIM-1165739

Modern Language Association (MLA)

Garro-Piña, Hazel…[et al.]. Evaluation of the Loading, Unloading, and Permanent Deformation of Newly Available Epoxy Resin Coated Ni-Ti Wires Using Self-Ligating Brackets. International Journal of Dentistry No. 2017 (2017), pp.1-8.
https://search.emarefa.net/detail/BIM-1165739

American Medical Association (AMA)

Garro-Piña, Hazel& Jiménez-Cervantes, María Cristina& Ondarza-Rovira, Ricardo& Justus, Roberto& García-López, Salvador. Evaluation of the Loading, Unloading, and Permanent Deformation of Newly Available Epoxy Resin Coated Ni-Ti Wires Using Self-Ligating Brackets. International Journal of Dentistry. 2017. Vol. 2017, no. 2017, pp.1-8.
https://search.emarefa.net/detail/BIM-1165739

Data Type

Journal Articles

Language

English

Notes

Includes bibliographical references

Record ID

BIM-1165739