Using the plate-creep test to determine the impact strength properties of concrete
Author
Source
Journal of Engineering Research
Issue
Vol. 10, Issue 4 B (31 Dec. 2022), pp.115-127, 13 p.
Publisher
Kuwait University Academic Publication Council
Publication Date
2022-12-31
Country of Publication
Kuwait
No. of Pages
13
Main Subjects
Abstract EN
The paper aims to design a concrete against repetitive impact and abrasion resistance.
macro/micro steel fibers and two types of crushed stone based on limestone and corundum as aggregate were used in concrete mixtures.
impact test device has been modified, designed, and used for impact strength testing of concrete.
the usability of the plate-creep test in determining the impact strength of concrete was also investigated.
according to the test results, a high correlation was found between the abrasion, impact resistance tests, and the creep test.
American Psychological Association (APA)
Gokce, Murat. 2022. Using the plate-creep test to determine the impact strength properties of concrete. Journal of Engineering Research،Vol. 10, no. 4 B, pp.115-127.
https://search.emarefa.net/detail/BIM-1494630
Modern Language Association (MLA)
Gokce, Murat. Using the plate-creep test to determine the impact strength properties of concrete. Journal of Engineering Research Vol. 10, no. 4 B (Dec. 2022), pp.115-127.
https://search.emarefa.net/detail/BIM-1494630
American Medical Association (AMA)
Gokce, Murat. Using the plate-creep test to determine the impact strength properties of concrete. Journal of Engineering Research. 2022. Vol. 10, no. 4 B, pp.115-127.
https://search.emarefa.net/detail/BIM-1494630
Data Type
Journal Articles
Language
English
Notes
Includes bibliographical references : p. 126-127
Record ID
BIM-1494630