The activation controlled galvanic corrosion of carbon steel zinc couple in deaerated stirred 0.2 N HCl
Joint Authors
Said, Farqad F. M.
Sulayman, Qasim Jasim Muhammad
Source
Journal of Saudi Chemical Society
Issue
Vol. 9, Issue 2 (30 Sep. 2005), pp.437-447, 11 p.
Publisher
Publication Date
2005-09-30
Country of Publication
Saudi Arabia
No. of Pages
11
Main Subjects
Topics
Abstract AR
تمت دراسة تأثير الربط الجلفاني لمعدني الفولاذ الكربوني و الخارصين في محلول 0,2 عياري من حمض كلوريد الهيدروجين باستخدام تقنية مقياس التيار ذي المقاومة الصفرية المتعدد لقياس التيار الجلفاني (Ig) و جهد الربط (Ecop.) مقابل الزمن.
و تبين أن لتغيير نسبة مساحة المهبط / المصعد (0,5 إلى 2) و زيادة درجة الحرارة (GF)، التيار الجلفاني (Ig) و تيار الذوبان (Id) في معظم الحالات.
Abstract EN
The effect of galvanic coupling of carbon steel to zinc (C.S.
/ Zn) in DE aerated 0.2 N HCl was studied using the multiple zero resistance technique to measure the galvanic current (Ig) and the coupling potential (Ecop,) versus time for the coupled metals.
It was found that altering area ratio (AR) (Cathode / Anode) of the coupled metals and increasing temperature played an important role in increasing corrosion rate as well as changing the galvanic factor (GF), galvanic current (Ig), and dissolution current (Id), in most of the cases.
American Psychological Association (APA)
Said, Farqad F. M.& Sulayman, Qasim Jasim Muhammad. 2005. The activation controlled galvanic corrosion of carbon steel zinc couple in deaerated stirred 0.2 N HCl. Journal of Saudi Chemical Society،Vol. 9, no. 2, pp.437-447.
https://search.emarefa.net/detail/BIM-26409
Modern Language Association (MLA)
Said, Farqad F. M.& Sulayman, Qasim Jasim Muhammad. The activation controlled galvanic corrosion of carbon steel zinc couple in deaerated stirred 0.2 N HCl. Journal of Saudi Chemical Society Vol. 9, no. 2 (Sep. 2005), pp.437-447.
https://search.emarefa.net/detail/BIM-26409
American Medical Association (AMA)
Said, Farqad F. M.& Sulayman, Qasim Jasim Muhammad. The activation controlled galvanic corrosion of carbon steel zinc couple in deaerated stirred 0.2 N HCl. Journal of Saudi Chemical Society. 2005. Vol. 9, no. 2, pp.437-447.
https://search.emarefa.net/detail/BIM-26409
Data Type
Journal Articles
Language
English
Notes
Includes bibliographical references : p. 446-447
Record ID
BIM-26409