Objectives : this study evaluated the effect of reinforcing high-impact acrylic resin (Metrocryl HI) with zirconia powder in two different concentrations on the transverse strength, impact strength, surface hardness, water sorption and solubility.

Materials and methods : Fifteen specimens were prepared for each test, five from Metrocryl HI resin as control, five others were prepared from the 5 % zirconia-modified Metrocryl HI resin, and another five specimens were prepared from the 15 % zirconia-modified Metrocryl HI resin.

Transverse strength was assessed with a 3-point bending test using a screw-driven testing machine.

For the impact strength, a Charpy tester was used.

Surface hardness testing was conducted using Vickers tester.

The water sorption and solubility test was performed according to International Standards Organization specification No.

1567 for denture base polymers.

Micro-structural examination of two specimens, one representing each ZrO2 concentration group, was carried out using scanning electron microscopy.

Results : as determined by ANOVA and Bonferroni multiple comparison tests, the addition of zirconia resulted in a highly significant increase in transverse strength of high-impact acrylic resin (P < 0.001).

This increase was proportional to the concentration of zirconia.

No significant difference was detected in each of impact strength, surface hardness and water solubility (P > 0.05).

Although a significant increase in water sorption was demonstrated (P < 0.05), still its mean value lies within the specification limits.

Conclusions : reinforcement of high-impact acrylic resin with zirconia powder increases its transverse strength significantly.

American Psychological Association (APA)

Iyad, Nifin M.& Badawi, Manal F.& Fattah, Abdu A.. 2008. The Effect of reinforcementof high-impact acrylic resin with zirconia on some physical and mechanical properties. Cairo Dental Journal،Vol. 24, no. 2, pp.245-250.
https://search.emarefa.net/detail/BIM-276111

Modern Language Association (MLA)

Iyad, Nifin M.…[et al.]. The Effect of reinforcementof high-impact acrylic resin with zirconia on some physical and mechanical properties. Cairo Dental Journal Vol. 24, no. 2 (May. 2008), pp.245-250.
https://search.emarefa.net/detail/BIM-276111

American Medical Association (AMA)

Iyad, Nifin M.& Badawi, Manal F.& Fattah, Abdu A.. The Effect of reinforcementof high-impact acrylic resin with zirconia on some physical and mechanical properties. Cairo Dental Journal. 2008. Vol. 24, no. 2, pp.245-250.
https://search.emarefa.net/detail/BIM-276111

Data Type

Journal Articles

Language

English

Notes

Includes bibliographical references : p. 250

Record ID

BIM-276111