Carbonization and treatment the high temperature distortion of thoriated tungsten cathode for high power electronic tubes

Other Title(s)

كربنة و معالجة تشوه كاثود التنكستن المطعم بالثوريا عند درجات الحرارة العالية للصمامات الإلكترونية العالية القدرة

Joint Authors

al-Basam, Fadil Abbas Hashim Muhammad
Rauf, Waddah Jamil
Faisal, Abd al-Qadir Dawud

Source

Baghdad Science Journal

Issue

Vol. 6, Issue 4 (31 Dec. 2009), pp.763-769, 7 p.

Publisher

University of Baghdad College of Science for Women

Publication Date

2009-12-31

Country of Publication

Iraq

No. of Pages

7

Main Subjects

Engineering & Technology Sciences (Multidisciplinary)

Topics

Abstract AR

يهدف البحث إلى تشكيل و كربنة و معالجة التشوهات الناتجة بعد الكربنة لكاثودات الصمامات الإلكترونية ذات القدرة العالية.

لقد تم إجراء دراسة لتصميم قوالب لتصنيع الكاثودات الخاصة بالصمام الإلكتروني الرباعي المستخدم في منظومات الإرسال الإذاعي من نوع (TH558) كذلك صممت و صنعت منظومة لكربنة الكاثودات المصنعة كدالة لدرجة الحرارة و الضغط و الزمن و التيار و الفولتية.

كربنت أسلاك التنكستن المطعم بالثوريا مختلفة الأقطار لتحديد المتغيرات الخاصة بعملية الكربنة.

تم دراسة عملية تشوهات الكاثودات الناتجة بعد إجراء عملية الكربنة و تحديد طرق معالجتها ضمن الحدود الدنيا لكل من قيم درجة الكربنة و انحرافات التشوهات.

تم إجراء عمليات القياس الدقيق للتشوهات الحاصلة للكاثود المكربن كدالة لدرجات الحرارة التي تتراوح بين (1800 – 1500) ˚م.

لقد تم تحديد درجات الحرارة باستخدام البايروميتر الضوئي عمليا و تطبيق معادلة ستيفان – بولتزمان نظريا.

Abstract EN

A metal mandrel was designed for manufacturing the cathodes of high power electron tube ( Tetrode ) used in broadcasting transmitting tubes type TH558 and CQS200.The cathodes were manufactured in the present work from thoriated tungsten wires ( 2٪ ThO2- W) with different diameters .These cathodes were carbonized in sequences of processes to determine the carbonization parameters (temperature, pressure, time, current and voltage).Then the carbonized cathodes dimension were accurately measured to determine the deviation due to the high temperature distortion effect at about 1800°C .the distorted cathodes due to the carbonization process was treated when it was subjected inside the vacuum chamber and heat treated again .The carbonized cathode distortions as a function of temperature were measured in the range of (1500°C-1800°C).The temperature was determined using an optical pyrometer and also calculated using Stephan's-Boltzmann relation.

American Psychological Association (APA)

Faisal, Abd al-Qadir Dawud& al-Basam, Fadil Abbas Hashim Muhammad& Rauf, Waddah Jamil. 2009. Carbonization and treatment the high temperature distortion of thoriated tungsten cathode for high power electronic tubes. Baghdad Science Journal،Vol. 6, no. 4, pp.763-769.
https://search.emarefa.net/detail/BIM-353945

Modern Language Association (MLA)

Faisal, Abd al-Qadir Dawud…[et al.]. Carbonization and treatment the high temperature distortion of thoriated tungsten cathode for high power electronic tubes. Baghdad Science Journal Vol. 6, no. 4 (Dec. 2009), pp.763-769.
https://search.emarefa.net/detail/BIM-353945

American Medical Association (AMA)

Faisal, Abd al-Qadir Dawud& al-Basam, Fadil Abbas Hashim Muhammad& Rauf, Waddah Jamil. Carbonization and treatment the high temperature distortion of thoriated tungsten cathode for high power electronic tubes. Baghdad Science Journal. 2009. Vol. 6, no. 4, pp.763-769.