![](/images/graphics-bg.png)
Exfoliation Corrosion and Pitting Corrosion and Their Role in Fatigue Predictive Modeling : State-of-the-Art Review
Joint Authors
Arriscorreta, Carlos A.
Hoeppner, David W.
Source
International Journal of Aerospace Engineering
Issue
Vol. 2012, Issue 2012 (31 Dec. 2012), pp.1-29, 29 p.
Publisher
Hindawi Publishing Corporation
Publication Date
2012-02-09
Country of Publication
Egypt
No. of Pages
29
Main Subjects
Engineering Sciences and Information Technology
Abstract EN
Intergranular attack (IG) and exfoliation corrosion (EC) have a detrimental impact on the structural integrity of aircraft structures of all types.
Understanding the mechanisms and methods for dealing with these processes and with corrosion in general has been and is critical to the safety of critical components of aircraft.
Discussion of cases where IG attack and exfoliation caused issues in structural integrity in aircraft in operational fleets is presented herein along with a much more detailed presentation of the issues involved in dealing with corrosion of aircraft.
Issues of corrosion and fatigue related to the structural integrity of aging aircraft are introduced herein.
Mechanisms of pitting nucleation are discussed which include adsorption-induced, ion migration-penetration, and chemicomechanical film breakdown theories.
In addition, pitting corrosion (PC) fatigue models are presented as well as a critical assessment of their application to aircraft structures and materials.
Finally environmental effects on short crack behavior of materials are discussed, and a compilation of definitions related to corrosion and fatigue are presented.
American Psychological Association (APA)
Hoeppner, David W.& Arriscorreta, Carlos A.. 2012. Exfoliation Corrosion and Pitting Corrosion and Their Role in Fatigue Predictive Modeling : State-of-the-Art Review. International Journal of Aerospace Engineering،Vol. 2012, no. 2012, pp.1-29.
https://search.emarefa.net/detail/BIM-453268
Modern Language Association (MLA)
Hoeppner, David W.& Arriscorreta, Carlos A.. Exfoliation Corrosion and Pitting Corrosion and Their Role in Fatigue Predictive Modeling : State-of-the-Art Review. International Journal of Aerospace Engineering No. 2012 (2012), pp.1-29.
https://search.emarefa.net/detail/BIM-453268
American Medical Association (AMA)
Hoeppner, David W.& Arriscorreta, Carlos A.. Exfoliation Corrosion and Pitting Corrosion and Their Role in Fatigue Predictive Modeling : State-of-the-Art Review. International Journal of Aerospace Engineering. 2012. Vol. 2012, no. 2012, pp.1-29.
https://search.emarefa.net/detail/BIM-453268
Data Type
Journal Articles
Language
English
Notes
Includes bibliographical references
Record ID
BIM-453268