Susceptibility to Stress Corrosion of Laser-Welded Composite Arch Wire in Acid Artificial Saliva
Joint Authors
Source
Advances in Materials Science and Engineering
Issue
Vol. 2013, Issue 2013 (31 Dec. 2013), pp.1-8, 8 p.
Publisher
Hindawi Publishing Corporation
Publication Date
2013-06-13
Country of Publication
Egypt
No. of Pages
8
Main Subjects
Engineering Sciences and Information Technology
Abstract EN
The corrosion resistance of laser-welded composite arch wire (CoAW) with Cu interlayer between NiTi shape memory alloy and stainless steel wire in artificial saliva with different acidities and loads was studied.
It was found that both the solution pH and the stress had a significant influence on the corrosion behaviors of the CoAW samples.
Decreasing the solution pH or increasing the loading stress caused the increase of Cu release and weight loss.
The corroded morphology formed on the surfaces of the CoAW was the consequence under the combined effect of corrosion and stress.
American Psychological Association (APA)
Zhang, Chao& Sun, Xinhua. 2013. Susceptibility to Stress Corrosion of Laser-Welded Composite Arch Wire in Acid Artificial Saliva. Advances in Materials Science and Engineering،Vol. 2013, no. 2013, pp.1-8.
https://search.emarefa.net/detail/BIM-494811
Modern Language Association (MLA)
Zhang, Chao& Sun, Xinhua. Susceptibility to Stress Corrosion of Laser-Welded Composite Arch Wire in Acid Artificial Saliva. Advances in Materials Science and Engineering No. 2013 (2013), pp.1-8.
https://search.emarefa.net/detail/BIM-494811
American Medical Association (AMA)
Zhang, Chao& Sun, Xinhua. Susceptibility to Stress Corrosion of Laser-Welded Composite Arch Wire in Acid Artificial Saliva. Advances in Materials Science and Engineering. 2013. Vol. 2013, no. 2013, pp.1-8.
https://search.emarefa.net/detail/BIM-494811
Data Type
Journal Articles
Language
English
Notes
Includes bibliographical references
Record ID
BIM-494811