تصنيع حراريات مسامية من خام الكاؤلين العراقي بإضافة عجينة الورق التالف
Other Title(s)
Manufacturing porous ceramic from Iraqi kaolin by using paper pulp
Joint Authors
Source
Issue
Vol. 35, Issue (s1) (31 Dec. 2017), pp.227-236, 10 p.
Publisher
Publication Date
2017-12-31
Country of Publication
Iraq
No. of Pages
10
Main Subjects
Natural & Life Sciences (Multidisciplinary)
Abstract EN
In this work porous clay refractory was prepared from Iraqi kaolin clay; by addition of water or different type of paper pulp; the paper pulp different in (paper : water), the sample formed by mold method, then dried at room temperature for (72) hr at last fired at (1200)oC with soaking time for (2) hr.
Properties (linear shrinkage, loss in mass, apparent porosity, water absorption ratio, apparent density, thermal conductivity, thermal shook resistance and diametrical strength) were studied.
American Psychological Association (APA)
هادي، ي. م. وعبد الحسين، ج. ه.. 2017. تصنيع حراريات مسامية من خام الكاؤلين العراقي بإضافة عجينة الورق التالف. مجلة الهندسة والتكنولوجيا،مج. 35، ع. (s1)، ص ص. 227-236.
https://search.emarefa.net/detail/BIM-877926
Modern Language Association (MLA)
هادي، ي. م. وعبد الحسين، ج. ه.. تصنيع حراريات مسامية من خام الكاؤلين العراقي بإضافة عجينة الورق التالف. مجلة الهندسة والتكنولوجيا مج. 35، العدد الخاص الأول (2017)، ص ص. 227-236.
https://search.emarefa.net/detail/BIM-877926
American Medical Association (AMA)
هادي، ي. م. وعبد الحسين، ج. ه.. تصنيع حراريات مسامية من خام الكاؤلين العراقي بإضافة عجينة الورق التالف. مجلة الهندسة والتكنولوجيا. 2017. مج. 35، ع. (s1)، ص ص. 227-236.
https://search.emarefa.net/detail/BIM-877926
Data Type
Journal Articles
Language
Arabic
Notes
يتضمن مراجع ببليوجرافية : ص. 235-236
Record ID
BIM-877926